For getting better result of weld, it is necessary to control fully pressure force put in between electrodes which is one of the three important factors for welding conditions.
For getting better result of weld, it is necessary to control fully pressure force put in between electrodes which is one of the three important factors for welding conditions.
Model | SP-233SN | SP-236N | SP-231N | SP-233-3T | SP-233-3T | SP-233-4T | SP-241N | |
---|---|---|---|---|---|---|---|---|
Range | 0.3~3kN | 0.6~6kN | 1~10kN | 2~20kN | 3~30kN | 4~40kN | 1~10kN | |
Min.Scale | 100N(10kgf) | 200N(20kgf) | 200N(20kgf) | 200N(20kgf) | 1kN(100kgf) | 1kN(100kgf) | 200N(20kgf) | |
Accuracy | ±3% of Full Scale | |||||||
Weight (g) | Unit | 400 | 420 | 480 | 680 | 900 | 900 | 560 |
Case | 400 | 660 |
Model | SP-2010 | SP-2020 |
---|---|---|
Range | 0.5~10.0kgf | 1.0~20.0kgf |
Min.Scale | 0.1kgf | 0.1kgf |
Accuracy | ±3% of Full Scale | |
Weight | 470g | 470g |